Carbon | S | ash | volatiles | moisture |
% | <% | |||
98.5 | 0.3 | 0.8 | 0.7 | 0.5 |
98.5 | 0.2 | 0.8 | 0.7 | 0.5 |
99 | 0.05 | 0.5 | 0.5 | 0.5 |
Size:0-2mm 1-5mm 4-20mm or customized
Recarburizer Introduction
Recarburizer, also know as carbon additive, carbon raiser. It is a product for increasing the carbon element (C).
Recarburizer is quality material as reductive agent and carbon addictive in steelmaking, with the characteristics of high recovery rate, low sulfur and phosphorus content, no pollution. It is divided into ordinary carburizer and graphite carburizer. According to different smelting processes, carbon can be added during steel making and casting to increase the strength of steel and casting.
Recarburizer used in casting, can greatly increase the dosage of scrap steel, reduce the dosage of pig iron or no iron. Electric furnace smelting way of feeding, recarburizer with scrap steel should be burden to put together, such as small doses of adding can choose to add in the hot metal surface. But want to avoid mass feeding into the molten iron, in order to prevent excessive oxidation by carbonization effect is not obvious and the carbon content of the casting is not enough. Increased carbon agent, the dosage according to the ratio of other raw materials and carbon content. Different kinds of cast iron, according to need to choose different types of recarburizer. Choose recarburizer characteristics itself pure carbon graphite material, reduce too much impurity in the iron, carburant choose appropriate which can reduce the cost of castings.
Recarburizer features
1. High Carbon Levels
Our carbon levels can reach in the excess of 99% providing maximum cost efficiency. High carbon recovery ensures lower material consumption and processing time.
2. Low Sulfur
Our Carbon Additives is naturally low in Sulfur reducing costly post melting sulfur treatments.
3. Low Ash & Moisture Levels
Less slag formation due to our inherent low ash and moisture content resulting in better cast quality and productivity.
4. High Thermal & Electrical Conductivity
High Thermal & Electrical Conductivity ensure high dissolution rate resulting in higher production efficiencies and lower operating cost.
5. Quality Assured
Manufactured to our highest quality control to guarantee consistent cast quality and cost.